Design of Equipment and Operation of Laboratory Test for Heat Transfer Surface Inhibition in Cooling Water

A. J. Freedman, W. J. Ryzner, J. D. Knapp

Abstract

1963 Volume 12 Issue 10 Pages 478-483 in Japanese. Available at https://doi.org/10.3323/jcorr1954.12.10_478

Abstract Corrosion inhibitors in open recirculating cooling water systems require rapid and complete film formation for maximum effectiveness. The protective film is established on clean surfaces by initial treatment with inhibitor at high dosage levels. Protection then can be maintained by continuous treatment at substantially lower levels. If operational difficulties should cause loss of the protective film, low level treatment after the film has been lost may result in severely increased corrosion and deposition. Laboratory corrosion, deposition and consumption studies with polyphosphate-based and chromate-based inhibitors illustrate the advantages of high level start-up and low level maintenance treatments. These data are confirmed by actual field experiences. 5.8.1

Please sign in
to download the full paper.
Not registered yet? Follow this link
By registering, you agree to receive communications from Arthur Freedman Associates. You may opt-out at any time.
Arthur Freedman Associates
Privacy Overview

This website uses cookies so that we can provide you with the best user experience possible. Cookie information is stored in your browser and performs functions such as recognising you when you return to our website and helping our team to understand which sections of the website you find most interesting and useful.